Standard |
Correlative |
Composition(by mass)/% |
Melting |
Woking Temp.Min |
Characteristic & Application |
DIN | AWS |
Cu |
P |
Ag |
Other |
Sol. |
Liq. |
BCu91PAg |
|
BCuP-6 |
Rem. |
6.8-7.2 |
1.8-2.2 |
|
643 |
788 |
740 |
Brazing the joints of copper and copper alloy with larger gap,widely used for refrigeration,electromechanical and instrument etc industries |
BCu89PAg |
CP-104 |
BCuP-3 |
Rem. |
5.8-6.2 |
4.8-5.2 |
|
645 |
815 |
710 |
Good plasticity,low phosphorus conetent,it can braze the joints of copper and copper alloy with larger gap |
BCu88PAg |
|
BCuP-7 |
Rem. |
6.5-7.0 |
4.8-5.2 |
|
643 |
771 |
710 | Good plasticity,phosphorus content is higher than BCu89PAg,good fluidity,it can braze the joints of copper and copper alloy with smaller gap. |
BCu87PAg |
|
BCuP-4 |
Rem. |
7.0-7.5 |
5.8-6.2 |
|
643 |
813 |
720 |
BCu80AgP |
|
BCuP-5 |
Rem. |
4.8-5.2 |
14.5-15.5 |
|
645 |
800 |
700 | Higher plasticity and conductivity,braze the joints with larger gap and demanding conductivity. |